CONDUCTIVE (Anti-Static) AND NON-CONDUCTIVE
Conductive (Anti-Static)
Fiber |
N/A Multifilament Stainless Steel Polyester |
Retention |
N/A 5-10 microns |
Porosity1 | N/A 20 - 30 CFM |
Weave |
N/A 4 x 4 Twill |
Acids |
N/A Good resistance to most mineral and organic acids except high concentrations of nitric, sulfuric and carbolic acids. |
Alkalis |
N/A Good resistance to weak alkalis and moderate resistance to strong alkalis at low temperatures. Strong alkalis at high concentrations and temperatures dissolve polyesters. |
Oxidizing Agents |
N/A Good resistance to most oxidizing agents. |
Organic Solvents |
N/A Excellent to most organic solvents, but unsuited for some phenolic compounds and affected by cyclohexanone at 313 ºF. |